Steels low-alloy Gas-shielded ER90S-G logam Jointing barang
KOMPONEN KIMIA:
PADUNGAN (wt%) | C | Mn | Si | Cr | Ni | Mo | P | S | Cu |
ATURAN GB/T | 0.12 | 0.75-1.50 | 0.30-0.90 | 2.10-2.70 | - | 0.90-1.20 | 0.03 | 0.03 | 0.40 |
ATURAN AWS | - | - | - | - | - | - | - | - | - |
NILAI CONTOH | 0,075 | 0.85 | 0.60 | 2.5 | 0.03 | 1.00 | 0.01 | 0,005 | 0.05 |
PILIHAN MEKANIKAL:
HARTA | Kakuatan ngahasilkeun (MPa) | Kakuatan éksténsif (MPa) | NILAI IMPAK J/℃ | ELONGATION(%) | perlakuan panas °Cxh | |||||
ATURAN GB/T | 540 | 620 | - | 15 | 690*1 | |||||
ATURAN AWS | 540 | 620 | - | 17 | 690*1 | |||||
NILAI CONTOH | 560 | 640 | 160/0Suhu kamar | 24 | 690*1 |
Parameter las anu disarankeun:
SPESIFIKASI DIAMETER (mm) | 1.0 | 1.2 | 1.6 | |||||||
LISTRIK (Amp) | H/W | 50-220 | 80-350 | 170-550 | ||||||
O/W | 50-120 | 80-150 | - |
Gas shielded kawat las pikeun kelas baja tahan panas 620MPa.
Kawat lemes, busur stabil, molding geulis, beusi molten alus, téhnologi las alus teuing.
Logam molten miboga sipat mékanis alus, boga résistansi porosity alus sarta weld ngabentuk.
KOMPONEN KIMIA:
PADUNGAN (wt%) | C | Mn | Si | Cr | Ni | Mo | P | S | Cu |
ATURAN GB/T | 0.12 | 0.75-1.50 | 0.30-0.90 | 2.10-2.70 | - | 0.90-1.20 | 0.03 | 0.03 | 0.40 |
ATURAN AWS | - | - | - | - | - | - | - | - | - |
NILAI CONTOH | 0,075 | 0.85 | 0.60 | 2.5 | 0.03 | 1.00 | 0.01 | 0,005 | 0.05 |
PILIHAN MEKANIKAL:
HARTA | Kakuatan ngahasilkeun (MPa) | Kakuatan éksténsif (MPa) | NILAI IMPAK J/℃ | ELONGATION(%) | perlakuan panas °Cxh | |||||
ATURAN GB/T | 540 | 620 | - | 15 | 690*1 | |||||
ATURAN AWS | 540 | 620 | - | 17 | 690*1 | |||||
NILAI CONTOH | 560 | 640 | 160/0Suhu kamar | 24 | 690*1 |
Parameter las anu disarankeun:
SPESIFIKASI DIAMETER (mm) | 1.0 | 1.2 | 1.6 | |||||||
LISTRIK (Amp) | H/W | 50-220 | 80-350 | 170-550 | ||||||
O/W | 50-120 | 80-150 | - |
Tulis pesen anjeun di dieu sareng kirimkeun ka kami