alloy nikel MIG ERNiCrMo-3 Soldering makings
KOMPONEN KIMIA:
PADUNGAN (wt%) | C | Mn | Si | Cr | Ni | Mo | Fe | Nb+Ta | P | S |
ATURAN GB/T | 0.10 | 0.50 | 0.50 | 20.0-23.0 | ≥58 | 8.0-10.0 | 5.0 | 3.0-4.2 | - | - |
ATURAN AWS | 0.10 | 0.50 | 0.50 | 20.0-23.0 | ≥58 | 8.0-10.0 | 5.0 | 3.15-4.15 | 0.02 | 0.02 |
NILAI CONTOH | 0.006 | 0.15 | 0.15 | 22.01 | 64.80 | 8.72 | 0.18 | 3.49 | 0.001 | 0.001 |
PILIHAN MEKANIKAL:
HARTA | Kakuatan ngahasilkeun (MPa) | Kakuatan éksténsif (MPa) | NILAI IMPAK J/℃ | ELONGATION(%) | ||||
ATURAN GB/T | - | - | - | - | ||||
ATURAN AWS | - | - | - | - | ||||
NILAI CONTOH | - | 780 | 144/-196 | 45 |
Nikel-kromium-molybdenum nikel-base alloy gas kawat las, komposisi nominal nyaeta 61% Ni-22% Cr-9% Mo-3.5% Nb + Ta.
Sipat mékanis anu hadé sareng résistansi kana korosi pitting sareng crevice tina logam molten.
Nyoco kawat lemes, arc stabil, ngabentuk geulis, aliran alus logam panas, kirang Santika, kalawan kinerja prosés las alus teuing.
-
Cina Global demethane Tower
-
Zhejiang Petrokimia solar / tanki panyimpen minyak bumi
-
300.000-ton lepas pantai ngambang Produksi jeung Panyimpenan Tanker (FPSO)
KOMPONEN KIMIA:
PADUNGAN (wt%) | C | Mn | Si | Cr | Ni | Mo | Fe | Nb+Ta | P | S |
ATURAN GB/T | 0.10 | 0.50 | 0.50 | 20.0-23.0 | ≥58 | 8.0-10.0 | 5.0 | 3.0-4.2 | - | - |
ATURAN AWS | 0.10 | 0.50 | 0.50 | 20.0-23.0 | ≥58 | 8.0-10.0 | 5.0 | 3.15-4.15 | 0.02 | 0.02 |
NILAI CONTOH | 0.006 | 0.15 | 0.15 | 22.01 | 64.80 | 8.72 | 0.18 | 3.49 | 0.001 | 0.001 |
PILIHAN MEKANIKAL:
HARTA | Kakuatan ngahasilkeun (MPa) | Kakuatan éksténsif (MPa) | NILAI IMPAK J/℃ | ELONGATION(%) | ||||
ATURAN GB/T | - | - | - | - | ||||
ATURAN AWS | - | - | - | - | ||||
NILAI CONTOH | - | 780 | 144/-196 | 45 |